SAE AMS6478B Digital PDF

$48.00

Steel, Bars and Forgings, 3.1Cr – 11.5Ni – 13.5Co – 1.2Mo (0.21 – 0.25C), Vacuum Melted, Annealed, Heat Treatable to 290 ksi (1999 MPa) Tensile Strength
standard by SAE International, 09/30/2005

Document Format: PDF

Description

This specification covers a premium aircraft-quality alloy steel in the form of bars, forgings, and forging stock.

These products have been used typically for parts requiring a combination of high strength, high toughness, and weldability, but usage is not limited to such applications. Product after proper heat treatment should attain a minimum tensile strength of 290 ksi (1999 MPa) and yield strength of 245 ksi (1689 MPa).

Product Details

Published:
09/30/2005
File Size:
1 file , 100 KB
Note:
This product is unavailable in Ukraine, Russia, Belarus